High dimensional stability for complex shapes and thin walls
Good corrosion resistance
Good mechanical properties
High thermal and electrical conductivity
Great strength at high temperatures
Aluminum is cast at a temperature of 650 ºC (1200 ºF). It is alloyed with Silicon 9% and Copper about 3.5% to form the Aluminum Association 380 alloy (UNS A03800). Silicon increases the melt fluidity, reduces machinability, Copper increases hardness and reduces the ductility. By greatly reducing the amount of Copper (less than 0.6%) the chemical resistance is improved; thus, AA 360 (UNS A03600) is formulated for use in marine environments. A high silicon alloy is used in automotive engines for cylinder castings, AA 390 (UNS A03900) with 17% Silicon for high wear resistance.
High Pressure Die Casting :
In this process, the liquid metal is injected at high speed and high pressure into a metal mould. A schematic view of high pressure die casting is given in this figure.